Hot cracking
2 cases · 7 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00173 / May.2021
Welding Cracks in an Aged HP Cast Fitting
M - Heat Resistant SteelP - Cast FtittingAp - PetrochemicalCd - Welding
Cm - Kalling Etched Micrography by OMDf - Hot cracking

ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - NItal Etched MacroDf - Hot cracking
More from these cases

ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking

ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking

ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking

ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - Nital Etched Micrography by OMDf - Hot cracking

ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking