Welded Joint

3 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00149 / Dec.2018
Vibration Induced Fatigue in a Gas Piping
M - Low Carbon SteelP - Piping spoolAp - FPSOCd - Vibration Induced Fatigue
Cm - Aspect Before AnalysisDf - Welded Joint
ML00133 / May.2018
Seam Welded Pipe Cladded with Alloy 625
M - LAS / Ni AlloyP - Longitudinal Seam Welded PipeAp - Oil and GasCd - Welding
Cm - Aspect Before AnalysisDf - Welded Joint
The 4 1/2" nominal diameter seamless pipe  internally overlaid with Alloy 625. This pipe corresponds to a 90° curve. The overlaid pipe was heat treated before and after bending.  The final quenching and tempering heat treatment was conducted to meet API 5L X70 properties.
113
ML00132 / May.2018
Seamless Pipe Overlaid with Alloy 625
M - LAS / Ni AlloyP - Seamless PipeAp - Oil and GasCd - Welding
Cm - Aspect Before AnalysisDf - Welded Joint