Transverse Section

3 cases · 7 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - As polished micrographyDf - Transverse Section
ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Transverse Section
ML00076 / Jun.2017
Hydrogen Cracking of a 17-7 PH Subsea Spring
M - Precipitation Hardened Stainless SteelP - WireAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Transverse Section

More from these cases

ML00143 — Impact of a .308 Winchester on A36 PlateM - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by OMDf - Transverse Section
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - As polished micrographyDf - Transverse Section
ML00135 — MIC of a Non Magnetic Drilling ToolM - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Transverse Section
ML00076 — Hydrogen Cracking of a 17-7 PH Subsea SpringM - Precipitation Hardened Stainless SteelP - WireAp - SubseaCd - Hydrogen Embrittlement
ML00076 / Jun.2017
Hydrogen Cracking of a 17-7 PH Subsea Spring
M - Precipitation Hardened Stainless SteelP - WireAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Transverse Section