Transverse Section
3 cases · 5 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - As polished micrographyDf - Transverse Section

ML00035 / Dec.2017
Carbon Steel L Shape
M - Low Carbon SteelP - Rolled ShapeAp - StructureCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - Transverse Section

ML00010 / Oct.2017
Cold Cracks in a Gouged Weld Metal
M - Low Alloy Low Carbon QTP - Rolled PlateAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Transverse Section
More from these cases

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by OMDf - Transverse Section

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - As polished micrographyDf - Transverse Section