Sampling and Analysis

6 cases · 14 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by SEMDf - Heat Affected Zone
ML00161 / Mar.2020
Brittle Fracture of a High Strength Socket
M - Medium Carbon Tool SteelP - ToolAp - Oil and GasCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece
ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Low Mag
Aspect of the fracture surface in low magnification, showing a flat aspect (associated to a fatigue fracture micromechanims) and a rough aspect (associated to a ductile fracture micromechanism).
167
ML00130 / Jun.2018
Fatigue Fracture of Overloaded Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
Cm - Fractography by SEMDf - General View
ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by SEMDf - Fusion Line

More from these cases

ML00182 — Brittle Fracture of a LAS Fixing RodM - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece
ML00161 — Brittle Fracture of a High Strength SocketM - Medium Carbon Tool SteelP - ToolAp - Oil and GasCd - Brittle Fracture
ML00161 / Mar.2020
Brittle Fracture of a High Strength Socket
M - Medium Carbon Tool SteelP - ToolAp - Oil and GasCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece
ML00142 — Impact of a .308 Winchester on AR500 PlateM - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00045 — Subsea Tubular F6NM Martensitic SSM - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by SEMDf - Base Metal
ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by SEMDf - Weld Metal