Crevice Corrosion in a Subsea System — Aspect Before Analysis

Sampling and Analysis — sub-branches

Shaft pinion presenting the bearing surface, with machining markes, from where the thermal spray layer was detached.  The diameter of the 880 mm long shaft in this region is about 75 mm.
426
ML00108 / Dec.2017
Thermal Spray Layer in a Pinion Shaft
M - High Strength Low AlloyP - ShaftAp - EngineCd - Coating Defect
Cm - Aspect Before AnalysisDf - General View