Welded Joint

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

External aspect of the 8" diameter pipe that suffered localized thinning and leakage associated to the welded regions.  The vertical weld is the pipe seam and the horizontal weld is the circunferential butt weld.
142
ML00005 / Apr.2017
Environmental Hydrogen Damage in Ti Pipe
M - Unalloyed TitaniumP - Longitudinal Seam Welded PipeAp - PipingCd - Hydride Formation
Cm - Aspect Before AnalysisDf - Welded Joint