Crevice Corrosion in a Subsea System — Aspect Before Analysis

The longitudinal section of the 1/2" thick pipe close to the washout position shows that the external tool marks are like notches that are corroded and cracks are iniciating from the corroded regions.  The top of the figure presents the external pipe surface and the bottom of the figure presents the internal pipe surface, with a green coating and the rusted washout.
154
ML00068 / Sep.2020
Corrosion Fatigue of a 5" Drill Pipe
M - Low Alloy Medium Carbon QTP - Seamless PipeAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - NItal Etched MacroDf - Longitudinal Section