Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - Aspect Before AnalysisDf - General View
General view of the nodular cast iron crankshaft, 240 mm long, in process of heat treatment.  The main and rod bearings, 54 mm diameter, are heat treated  by localized quenching and tempering.
1018
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Aspect Before AnalysisDf - General View
Aspect of the 5/8" diameter pin, that was 3" long and broke close to the center.
104
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Aspect Before AnalysisDf - General View