Close to the Internal Surface

2 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - FeCl3+HCl+Ethanol Etched MicroDf - Close to the Internal Surface
ML00044 / Feb.2017
Centrifugally Cast CuAl Bushing
M - Aluminum BronzeP - Cast BushingAp - EngineCd - Removed From Service
Cm - NH4OH+H2O+H2O2 Etched MicroDf - Close to the Internal Surface

More from these cases

ML00044 — Centrifugally Cast CuAl BushingM - Aluminum BronzeP - Cast BushingAp - EngineCd - Removed From Service
ML00044 / Feb.2017
Centrifugally Cast CuAl Bushing
M - Aluminum BronzeP - Cast BushingAp - EngineCd - Removed From Service
Cm - NH4OH+H2O+H2O2 Etched MicroDf - Close to the Internal Surface