Close to the Internal Surface

2 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00107 / Dec.2017
Carburized 9Cr1MoV Superheater Tube
M - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
Cm - As polished micrographyDf - Close to the Internal Surface
The micrography of the longitudinal section of the tube, close to ID, shows the paralel cracks, filled with oxides, perpendicular to the surface.
229
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - As polished micrographyDf - Close to the Internal Surface

More from these cases

ML00107 — Carburized 9Cr1MoV Superheater TubeM - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
ML00107 / Dec.2017
Carburized 9Cr1MoV Superheater Tube
M - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
Cm - Nital Etched Micrography by OMDf - Close to the Internal Surface