Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - As polished micrographyDf - Close to the External Surface

ML00060 / Apr.2017
Brittle Fracture of a Chilled Cast Iron Camshaft
M - Chilled Cast IronP - ShaftAp - AutomotiveCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Close to the External Surface
More from these cases

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Close to the External Surface

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - As polished micrographyDf - Close to the External Surface

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Close to the External Surface

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Close to the External Surface

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Close to the External Surface

ML00060 / Apr.2017
Brittle Fracture of a Chilled Cast Iron Camshaft
M - Chilled Cast IronP - ShaftAp - AutomotiveCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Close to the External Surface