Microstructure

2 cases · 4 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Microstructure — sub-branches

ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Decarburized Surface
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Martensite

More from these cases

ML00172 — Brittle Fracture of a LAS Valve SpringM - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Martensite
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Martensite