Coarse Structure

3 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure
Micrography of the flange in the longitudinal section. The flange microstructure is ferritic austenitic, presenting a coarse structure.
102
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure