Longitudinal Section
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Pitting Corrosion ×Microstructure: Austenite ×Capture method: Optical Microscope ×clear all

ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Longitudinal Section
More from these cases

ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Longitudinal Section