Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the broken bolt 1 1/2" nominal diameter, after a short time in service (non residente subsea equipment) under cathodic protection. The bolt broke at the thread fillet, close to the head.
800
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Aspect Before AnalysisDf - General View

More from these cases

ML00074 — Hydrogen Cracking of a 17-4 PH Subsea BoltM - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Fracture view presenting two diferente aspects, brittle in the bottom of the figure and in the center (most part of the fracture) and ductile in the top of the figure. Nominal diameter of the bolt 1 1/2".
203
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Fracture Surface AspectDf - General View