Crevice Corrosion in a Subsea System — Aspect Before Analysis

2" drain line from the main 10" line. The leakage occurred at the margin of the weld, a short time after the introduction of the reinforced ribs to reduce vibration.
641
ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Field photoDf - General View
The titanium rotor blade of a flowmeter broke after two years in service in an acid environment, containing H2S.
339
ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Aspect Before AnalysisDf - General View

More from these cases

ML00179 — Hydrides in Titanium WeldM - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Aspect Before AnalysisDf - General View