Fracture
11 cases · 13 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Fractography by SEMDf - Fracture

ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Fractography by SEMDf - Fracture

ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Fracture

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fracture

ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fracture

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Fracture

ML00138 / Jun.2018
Liquid Metal Embrittlement of a HSLA Steel
M - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
Cm - Fractography by SEMDf - Fracture

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Fracture
More from these cases

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Fracture

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Fracture