Welding Defect

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

The dye check image shows the detected crack, 50 mm long, at the margin of the weld in the forging side.
137
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Aspect by NDTDf - Cracking