Welding Defect
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Microstructure: Tempered Martensite ×Standard: grade F22 ×Capture method: Aspect Before Analysis ×clear all

ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Aspect Before AnalysisDf - General View
More from these cases

ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Aspect Before AnalysisDf - External Surface