Crevice Corrosion in a Subsea System — Aspect Before Analysis

The drilling connector, 21" diameter, presented a crack at the margin of the weld in the forging side (left side of the weld in the figure).
745
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Aspect Before AnalysisDf - General View
Fracture occurred during fabrication of a low carbon steel automotive part, welded by SAW process in one fillet, between a superior plate (8mm thick) and an inferior plate (12 mm thick). See the schematic drawing in the next figure.
290
ML00069 / May.2017
Liquation Cracks in SAW of Low Carbon Steel
M - Low Carbon SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Aspect Before AnalysisDf - Fracture
ML00072 / Jan.2018
Liquation Cracks in a High Strength Joint
M - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
Cm - Aspect Before AnalysisDf - General View
ML00067 / May.2017
Cold Cracks in C-Mn SAW Weld Metal
M - CMn SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Aspect Before AnalysisDf - Welded Joint

More from these cases

ML00178 — Cold cracks in Cr-Mo Welded ForgingM - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Circumferential weld aspect. Two passes in the cap. This forging to pipe welded joint, 22 mm thick, was welded by an automatic process in a narrow gap.  The pipe is to the top of the image and the forging is to the bottom of the image.
165
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Aspect Before AnalysisDf - External Surface
ML00067 — Cold Cracks in C-Mn SAW Weld MetalM - CMn SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
ML00067 / May.2017
Cold Cracks in C-Mn SAW Weld Metal
M - CMn SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Aspect Before AnalysisDf - Fracture