Crevice Corrosion in a Subsea System — Aspect Before Analysis
Damage — sub-branches

ML00072 / Jan.2018
Liquation Cracks in a High Strength Joint
M - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Weld Metal

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Root

ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched Micrography by OMDf - Weld Metal
More from these cases

ML00072 / Jan.2018
Liquation Cracks in a High Strength Joint
M - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Weld Metal

ML00072 / Jan.2018
Liquation Cracks in a High Strength Joint
M - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Weld Metal

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Root

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Center

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Center

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Cap

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Cap

ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched Micrography by OMDf - Weld Metal

ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched Micrography by OMDf - Weld Metal