Damage

2 cases · 4 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched Micrography by OMDf - Weld Metal
ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Weld Metal

More from these cases

ML00059 — Intergranular Corrosion of Aluminum PipingM - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched Micrography by OMDf - Weld Metal
ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched Micrography by OMDf - Weld Metal