Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - Kalling Etched MacroDf - Longitudinal Section

More from these cases

ML00094 — MIC of a Subsea Hydraulic LineM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior