Damage

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

Aspect of the broken bolt 1 1/2" nominal diameter, after a short time in service (non residente subsea equipment) under cathodic protection. The bolt broke at the thread fillet, close to the head.
800
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Aspect Before AnalysisDf - General View