Damage

1 case · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Micrography of the transverse section of the platesheet at the interface between the corroded and the non-corroded regions. The micrography is in the as polished condition.
140
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - As polished micrographyDf - Preferential Dissolution

More from these cases

ML00125 — Dezincification of a Cooler TubesheetM - BrassP - PlateAp - ShipCd - Preferential Dissolution
Micrography of the transverse section of the platesheet showing that part of the material (right side in the top of the figure) was lost (corroded).
129
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - As polished micrographyDf - Preferential Dissolution