Damage

3 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

General aspect of the 5/8" allen bolt that was found fractured in an instrument connected to a subsea BOP. The fracture presented a brittle aspect and occurred at the bolt head to threaded body transition.
1495
ML00139 / Jun.2018
Hydrogen Fracture of a 17-4 PH Allen Bolt
M - Precipitation Hardened Stainless SteelP - Allen BoltAp - SubseaCd - Hydrogen Embrittlement
Cm - Aspect Before AnalysisDf - Fracture
Aspect of the bolt fracture.  The fracture appearance is irregular.
137
ML00077 / Jun.2018
Hydrogen Cracking of LAS Subsea Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Aspect Before AnalysisDf - Fracture
ML00076 / Jun.2017
Hydrogen Cracking of a 17-7 PH Subsea Spring
M - Precipitation Hardened Stainless SteelP - WireAp - SubseaCd - Hydrogen Embrittlement
Cm - Aspect Before AnalysisDf - Fracture