Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Transverse Section AspectDf - Localized Thinning

More from these cases

ML00180 — Local Melting of Copper Cooling TubesM - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Transverse Section AspectDf - Leakage
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Transverse Section AspectDf - Thinning
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Transverse Section AspectDf - Leakage