Damage
1 case · 3 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Application: Ship ×Microstructure: Duplex Ferritic Austenitic ×Capture method: Scanning Electron Microscope ×clear all
Damage — sub-branches

ML00147 / Aug.2018
WC Layer Detached from a Cast Lean Duplex
M - Lean Duplex Stainless SteelP - Centrifugal CastingAp - ShipCd - Lack of Sealing
Cm - Electrolytic Etch Micrography by SEMDf - Thermal Spray Layer
More from these cases

ML00147 / Aug.2018
WC Layer Detached from a Cast Lean Duplex
M - Lean Duplex Stainless SteelP - Centrifugal CastingAp - ShipCd - Lack of Sealing
Cm - Electrolytic Etch Micrography by SEMDf - Thermal Spray Layer

ML00147 / Aug.2018
WC Layer Detached from a Cast Lean Duplex
M - Lean Duplex Stainless SteelP - Centrifugal CastingAp - ShipCd - Lack of Sealing
Cm - Electrolytic Etch Micrography by SEMDf - Sigma