Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

Aspect of the broken spring. The wire is 36 mm diameter and the ourter diameter of the spirals is 320 mm. It was broken in different locations.
434
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - General View

More from these cases

ML00172 — Brittle Fracture of a LAS Valve SpringM - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - Fracture
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - Corrosion
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - Brittle Fracture
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - General View