Damage
1 case · 5 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Damage — sub-branches

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Pearlite
More from these cases

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Strain Hardened

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Pearlite

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Strain Hardened

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Zn Layer