Corrosion

4 cases · 11 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Transgranular Cracking
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Transgranular Cracking
Low magnification micrography of the multiple cracks, parallel, transgranular. No evidences of microstrutural changes (heat evolution or decarburization).
127
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Transgranular Cracking
Micrography of a transverse section of the shell plate in a cracked position showing the transgranular morphology of the stress corrosion cracks.
167
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by SEMDf - Transgranular Cracking

More from these cases

ML00171 — Corrosion Fatigue of U Bolt Pipe ClampM - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Transgranular Cracking
ML00163 — Corrosion Fatigue of a Boiler Waterwall TubeM - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Micrography of the crack tip, initiated from the internal tube surface.  The crack is transgranular, filled with oxides and blunt-tipped.
109
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Transgranular Cracking
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Transgranular Cracking
ML00019 — Transgranular SCC in Boiler Steam DrumM - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Transgranular Crack
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Transgranular Crack
Micrographic detail of the transgranular stress corrosion cracking.
157
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Transgranular Crack
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by SEMDf - Transgranular Crack