Preferential Dissolution

3 cases · 6 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Internal Surface
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Corrosion
External surface aspect of the flange showing preferential dissolution, responsible for nucleation of the through wall cracking.
245
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Preferential Dissolution

More from these cases

ML00170 — MIC in Aluminum Brass TubesM - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Pitting
ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Corrosion
ML00002 — Preferential Dissolution and Cracks in SDSSM - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Detail of the region at the flange external surface where the material is suffering the preferential corrosion.
177
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Preferential Dissolution