Scanning Electron Microscope

5 cases · 18 images for “fracture”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Surface Aspect by SEMDf - Corrosion
ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Fractography by SEMDf - Fatigue Fracture
ML00093 / Sep.2017
MIC of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Heat Treated PartAp - O&G Well DrillingCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture

More from these cases

ML00182 — Brittle Fracture of a LAS Fixing RodM - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece
ML00172 — Brittle Fracture of a LAS Valve SpringM - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by SEMDf - Martensite
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by SEMDf - Martensite
ML00093 — MIC of a Drilling ToolM - Low Alloy Medium Carbon QTP - Heat Treated PartAp - O&G Well DrillingCd - Brittle Behavior
ML00093 / Sep.2017
MIC of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Heat Treated PartAp - O&G Well DrillingCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00093 / Sep.2017
MIC of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Heat Treated PartAp - O&G Well DrillingCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture
ML00093 / Sep.2017
MIC of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Heat Treated PartAp - O&G Well DrillingCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture
ML00080 — MIC of Stacking Disc SpringsM - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture