Crevice Corrosion in a Subsea System — Aspect Before Analysis
Scanning Electron Microscope — sub-branches

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece

ML00161 / Mar.2020
Brittle Fracture of a High Strength Socket
M - Medium Carbon Tool SteelP - ToolAp - Oil and GasCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Fractography by SEMDf - Close to the Internal Surface

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - At the Surface
More from these cases

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece

ML00161 / Mar.2020
Brittle Fracture of a High Strength Socket
M - Medium Carbon Tool SteelP - ToolAp - Oil and GasCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Fractography by SEMDf - In the Center of the Thickness

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Fractography by SEMDf - Close to the External Surface