Scanning Electron Microscope
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Application: Mechanical Industry ×Standard: D2 ×Detail focus: Close to the External Surface ×clear all
Scanning Electron Microscope — sub-branches

ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the External Surface
More from these cases

ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the External Surface