Fractography by SEM
8 cases · 22 images for “fatigue”
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Fracture

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fracture

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Crack

ML00050 / Nov.2017
Fatigue Failure of a 316SS Pressure Stabilizer
M - Austenitic Stainless SteelP - Fabrication WeldAp - Chemical IndustryCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture

ML00006 / Apr.2017
Vibration Induced Fatigue in 304SS
M - Austenitic Stainless SteelP - Longitudinal Seam Welded PipeAp - PipingCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Margin of the Weld Crack

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Fatigue Striation
More from these cases

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Close to the External Surface

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Dimples

ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Pitting

ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Pitting

ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture

ML00006 / Apr.2017
Vibration Induced Fatigue in 304SS
M - Austenitic Stainless SteelP - Longitudinal Seam Welded PipeAp - PipingCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00006 / Apr.2017
Vibration Induced Fatigue in 304SS
M - Austenitic Stainless SteelP - Longitudinal Seam Welded PipeAp - PipingCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Fatigue Striation