Fractography by SEM
3 cases · 14 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture

ML00093 / Sep.2017
MIC of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Heat Treated PartAp - O&G Well DrillingCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture

ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
More from these cases

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece

ML00093 / Sep.2017
MIC of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Heat Treated PartAp - O&G Well DrillingCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture

ML00093 / Sep.2017
MIC of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Heat Treated PartAp - O&G Well DrillingCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture

ML00093 / Sep.2017
MIC of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Heat Treated PartAp - O&G Well DrillingCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture

ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture

ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture

ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture

ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture