Fractography by SEM
4 cases · 16 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Dimples

ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture

ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Through Wall Cracking
More from these cases

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Elongated Dimples

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Elongated Dimples

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Dimples

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Elongated Dimples

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Ductile Fracture

ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture

ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Intergranular Cracking

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Fatigue Striation

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Fatigue Striation