Fractography by SEM

2 cases · 5 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

The hose connector fracture surface presented different fracture micromechanisms associated to the microstructure: inclusion decohesion, small regions of intergranular fractures (probably due to cementite at grain boundaries), and cleavage of the ferritic structure.  All these mechanisms are brittle.
560
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Brittle Fracture
ML00069 / May.2017
Liquation Cracks in SAW of Low Carbon Steel
M - Low Carbon SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Fractography by SEMDf - Intergranular Cracking

More from these cases

ML00103 — Brittle Fracture of a Free-Cutting ConnectorM - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Brittle Fracture
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture