Fractography by SEM

2 cases · 4 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Fractography by SEMDf - Plastic Deformation
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Ductile Fracture

More from these cases

ML00143 — Impact of a .308 Winchester on A36 PlateM - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Dimples
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Dimples