Fractography by SEM

3 cases · 6 images for “brittle fracture”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Fractography by SEMDf - Brittle Fracture
Detail of the fracture surface, predominantly transgranular with secondary cracks of intergranular morphology.
831
ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture
ML00075 / Jun.2018
Hydrogen Cracking of IN 718 Subsea Fasteners
M - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture

More from these cases

ML00174 — Carburization of a 347 SS Welded JointM - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Fractography by SEMDf - Brittle Fracture
ML00078 — Hydrogen Cracking of IN 718 Subsea ConnectorM - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture
ML00075 — Hydrogen Cracking of IN 718 Subsea FastenersM - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
ML00075 / Jun.2018
Hydrogen Cracking of IN 718 Subsea Fasteners
M - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture