ML00050 / Nov.2017
Fatigue Failure of a 316SS Pressure Stabilizer
M - Austenitic Stainless SteelP - Fabrication WeldAp - Chemical IndustryCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Striation