Fractography by SEM

1 case · 1 image for “fracture”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Fractographic analysis by scanning electron microscopy of the stud fracture surface after opening the cracks.  Brittle intergranular morphology with dimples and quasecleavage micromechanisms indicate that the internal cracks, intergranular, occurred by a hydrogen embrittlement effect during electroplating, and the ductile aspects are probably associated to overloading during torque.
517
ML00127 / May.2018
Hydrogen Cracks of Cadmium Plated Studs
M - Low Alloy Medium Carbon QTP - Allen StudAp - Oil and GasCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Fracture