Fractography by SEM
2 cases · 4 images for “embrittlement”
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00127 / May.2018
Hydrogen Cracks of Cadmium Plated Studs
M - Low Alloy Medium Carbon QTP - Allen StudAp - Oil and GasCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Fracture

ML00126 / Mar.2018
Hydrogen Fracture of Subsea Allen Bolts
M - Low Alloy Medium Carbon QTP - Coated ProductAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture
More from these cases

ML00127 / May.2018
Hydrogen Cracks of Cadmium Plated Studs
M - Low Alloy Medium Carbon QTP - Allen StudAp - Oil and GasCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking

ML00126 / Mar.2018
Hydrogen Fracture of Subsea Allen Bolts
M - Low Alloy Medium Carbon QTP - Coated ProductAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture