Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Fracture
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Fatigue Striation
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Fractography by SEMDf - Stress Corrosion Cracks
After opening the crack the fracture surface presented different aspects close to the internal surface and through the wall propagation.  Intergranular at the surface, showing intergranular SCC mechanism, and transgranular with striation, showing the contribution of pulsing loads.
101
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Through Wall Cracking
ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Fractography by SEMDf - Corrosion

More from these cases

ML00085 — Corrosion Fatigue of a Martensitic SS PinM - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Dimples
ML00165 — SCC of Aluminum Bronze Heating CoilM - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Fractography by SEMDf - Stress Corrosion Cracks
ML00011 — Intergranular SCC of Pure NickelM - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Intergranular Cracking
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Fatigue Striation
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion