Fractography by SEM

2 cases · 3 images for “fatigue”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Fractography by SEMDf - Fatigue Fracture
ML00081 / Aug.2017
Hydrogen Cracking of a Chromium Plated Carburized Pin
M - Low Alloy for Thermochemical TreatmentP - Chromium PlatedAp - AutomotiveCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Fatigue Striation

More from these cases

ML00081 — Hydrogen Cracking of a Chromium Plated Carburized PinM - Low Alloy for Thermochemical TreatmentP - Chromium PlatedAp - AutomotiveCd - Hydrogen Embrittlement
ML00081 / Aug.2017
Hydrogen Cracking of a Chromium Plated Carburized Pin
M - Low Alloy for Thermochemical TreatmentP - Chromium PlatedAp - AutomotiveCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Fatigue Striation