Fractography by SEM

1 case · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Fracture detail by scanning electron microscopy of the region where the cracking started, from the piping outside . The fracture is flat and shows fatigue striation.
138
ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

More from these cases

ML00150 — Vibration Induced Fatigue in a SS Oil PipingM - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Fracture detail by scanning electron microscopy of the region cloin the center of the thockness.  The fracture is flat and shows fatigue striation.
118
ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Striation