1 case · 1 image
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Atlas
/
Capture method
/
Scanning Electron Microscope
/ Fractography by SEM
Condition: Corrosion
×
Microstructure: Refined ferritic
×
clear all
Results
Sort
Newest
Oldest
Title A-Z
Title Z-A
42
VIEW
ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M
- Low Carbon Steel
P
- Bolt
Ap
- Ship
Cd
- Corrosion Fatigue
Cm
- Fractography by SEM
Df
- Fracture