Fractography by SEM
3 cases · 16 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture

ML00138 / Jun.2018
Liquid Metal Embrittlement of a HSLA Steel
M - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture

ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the External Surface
More from these cases

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece

ML00138 / Jun.2018
Liquid Metal Embrittlement of a HSLA Steel
M - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
Cm - Fractography by SEMDf - Zn Layer

ML00138 / Jun.2018
Liquid Metal Embrittlement of a HSLA Steel
M - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
Cm - Fractography by SEMDf - Fracture

ML00138 / Jun.2018
Liquid Metal Embrittlement of a HSLA Steel
M - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture

ML00138 / Jun.2018
Liquid Metal Embrittlement of a HSLA Steel
M - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking

ML00138 / Jun.2018
Liquid Metal Embrittlement of a HSLA Steel
M - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture

ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the Internal Surface

ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the Internal Surface

ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the External Surface